TEYING BUYER GUIDE · UPDATED OCTOBER 23, 2026
What EN 1811 Actually Tests on Your Finished Jewelry
EN 1811 measures the nickel that migrates off the worn, finished article rather than the nickel inside it — which is why a plated brass earring can pass and a "nickel-free" finding can fail. This covers the entry 27 limits and pass values, the EN 12472 wear simulation, and the report checks that separate evidence from decoration.

General guidance as of October 2026, not legal advice. Confirm limits and standard versions with your testing laboratory.
A release test, not a content test
Entry 27 of REACH Annex XVII sets the release ceilings: 0.5 µg/cm²/week for anything worn in direct and prolonged skin contact, 0.2 for posts that go into pierced body parts. EN 1811:2023, the harmonised test, judges results against pass values of 0.88 and 0.35. Where a piece is coated, EN 12472:2020 stands in for two years of wear first. What gets judged is the finished article as worn — not the alloy it was made from.
The reason the rule measures release instead of content is the allergy itself. Nickel allergy is contact dermatitis: nickel ions migrate from the surface onto the skin, usually carried by sweat. A content limit would be simpler for enforcement and would test the wrong thing.
Two consequences follow for buyers.
- Nickel inside the piece does not doom it. If the surface barrier survives wear, the piece passes — and the report, not the alloy certificate, is what proves that.
- And a nickel-free base does not save it. A nickel strike in the plating line, a nickel-bearing interlayer, or the wrong findings pulled from a parts bin can each push release over the line.
A spec sheet will not show either outcome. That is the argument for testing the finished design, not a similar piece from last season.
The two numbers to remember
Two ceilings, two pass values, and the pairing is easy to misquote.
For articles worn in direct and prolonged skin contact — earrings, necklaces, bracelets, rings, watch straps — the legal limit is 0.5 µg/cm²/week, and EN 1811:2023 treats a measured result of 0.88 or below as compliant. For post assemblies inserted into pierced body parts, the limit drops to 0.2 µg/cm²/week and the pass value to below 0.35.
Compliance at the 0.5 limit was reworded in the 2023 edition: 0.88 or below now passes, where the previous edition demanded strictly below 0.88. The 0.35 figure for piercing did not move. CEN published EN 1811:2023 on 22 February 2023, and it entered the harmonised list for entry 27 through Commission Communication C/2023/1604 that December, together with EN 12472:2020 and EN 16128:2015 for spectacle frames.
A report citing EN 1811:2011+A1:2015 is not wrong history — it is a superseded method. Ask for the current version.
Two years of wear, compressed into a week
Coated articles must hold release within the limit through at least two years of normal use, and EN 12472:2020 is the laboratory's approximation of those two years. The sequence: a corrosive atmosphere first, then tumbling with an abrasive paste and granules, and only after that the EN 1811 measurement.
Two details in the 2020 edition matter to buyers. The wear medium is now coconut shell granules alone — the earlier coconut-and-nut-shell mixture is gone — and the lactic acid reagent's purity floor rose from above 85 per cent to above 88 per cent. The second detail shapes designs: EN 12472 excludes articles whose outer coating itself contains nickel, because the standard will not fake protection a nickel-bearing top coating does not give. Where it is unclear whether the outer coating contains nickel, the accepted route is to run EN 1811 twice — with the wear simulation and without — and publish both results.
For a plated brass earring the plausible pass route is therefore a coating system with no nickel in the outer layer and a barrier that survives the tumbling barrel. Gold flash over a nickel interlayer is a familiar failure pattern — which is why the plating route belongs in the conversation before sampling, not after the first order.
What the finished-article rule rejects
Entry 27 reads the article as placed on the market, and EN 1811:2023 is explicit on two points: each sample tested must comply on its own, and sub-parts are assessed in their own right. In practice:
- A report on a brass blank, a loose finding or a plating coupon says nothing about the assembled earring.
- Post, hook, clasp, charm and any metal spacer that meets skin are each separate candidates.
- Swap the plating supplier, the thickness, the tumbling polish or the solder and the result can move, because each swap changes the surface that touches skin.
One report covering the material family rather than the SKU is an input, not evidence for the product you will sell.
Inside the lab: what your sample goes through
On the bench, the method runs in a fixed order.
First the lab picks out every part that sits in direct, prolonged skin contact, then decides whether the article is coated — and whether that outer coating contains nickel. A qualifying coating sends the piece through the EN 12472:2020 wear and corrosion simulation first. The test part then sits in artificial sweat solution per EN 1811 for one week at around 30 °C. Afterwards the nickel that leached into the solution is quantified, normally by ICP-OES or an equivalent method, divided by the exposed surface area measured before masking. Each part and each sample is published against the 0.88 or 0.35 pass value, in µg/cm²/week.
Sterling silver takes the same path: no automatic exemption, and rhodium-plated silver counts as coated, so it goes through the wear simulation like any other piece.
Reading a report: the checks that matter
Three groups of checks separate a usable report from decoration.
Identity. The report number and issue date — and whether the file is complete with its sample pages attached. The laboratory's name, address, and ISO/IEC 17025 accreditation listing EN 1811 within scope. Sample identification matching your SKU, batch and plating finish, with a photo where the laboratory provides one.
Method. The cited standard: EN 1811:2023, plus a statement of whether EN 12472:2020 was applied. Which parts were tested, and how the non-contact surfaces were masked.
Results. Per-sample, per-part figures in µg/cm²/week, printed beside the pass value instead of a bare pass mark. The margin to the limit — a result at 0.84 leaves nothing for production variation.
What TEYING confirms per project
A nickel-free requirement belongs in the brief before production, not in the inbox after sampling. Per design TEYING confirms the base material, the plating route and thickness range by SKU, the findings, and which test documentation can be provided for the destination market and order scope. Reports name the sample they were run on; when a design changes, the change is stated, so you can decide whether a retest is warranted.
That is the input a compliance file needs — not a standing certification. No factory statement replaces a report from an accredited laboratory on your specific production.
Put any nickel requirement into the brief and send it, with the target quantity, through the TEYING quote form.
FAQ
Does 925 silver need nickel testing?
Not automatically, but often. Entry 27 looks at the finished piece, not the alloy name on the spec — plating, solder and findings can each carry nickel into a silver item. Sterling content buys no exemption, because the measurement is what the surface releases; rhodium-plated silver runs the wear simulation like any other coated piece.
Can gold plated brass pass entry 27 if the brass has nickel?
In principle, yes, because the rule caps what is released rather than what is inside. Hold release at 0.5 µg/cm²/week or below after simulated wear and the piece passes — provided the outer coating itself is nickel-free. EN 12472's scope cannot rescue a nickel-bearing coating, so that design needs a different plating route.
Is an EN 1811:2011 report still acceptable?
It proves the same property on a method that has been replaced. The 2023 edition rewrote the acceptance wording and reworked its quality-control clauses, and buyers now expect that version. For a fresh production run, ask for EN 1811:2023 and have the report state whether EN 12472:2020 was applied.
What does "nickel free" mean on a spec sheet?
On most spec sheets it means the supplier intends to avoid nickel — not that a laboratory verified the finished piece. Ask whether the promise spans base alloy, plating route and findings, and get the report that ties the result to your SKU and batch.
Why does the test simulate two years of wear first?
Because entry 27 demands coated articles hold the limit through at least two years of normal use, and a fresh surface can hide what daily contact will expose. EN 12472:2020 compresses those two years into a corrosive exposure plus an abrasive tumble, run before the release measurement.
Have a nickel requirement attached to a design?
Put it in the brief: base material, plating route and the test documentation scope are confirmed per project.
Request a Factory Quote